PATHChat
SUBJECT: |
Autoclaved Aerated Concrete
|
FROM: |
CHEN CHIH CHIANG
taajan@ms10.hinet.net
|
DATE: |
2/5/1999 4:33:00 AM |
 |
|
In AAC(Autoclaved Aerated Concrete) production process, there always is a very nervous problem happened after
autoclaving procedure. The problem is the water mark(oval circle) on the surface of the AAC block. If there are any
people having this resolving experience or any idea for this, please mail me your advice to help me to improve this
problem.
|
 |
Partnership for Advancing Technology in Housing (PATH) 451 7th Street, SW, Rm. 8134 Washington, DC 20410-0001 Telephone: 202 708-4277 Fax: 202 708-4250 E-mail: pathnet@pathnet.org |
| |
|
|